We are seeing PCBs returned from our customer which have a black substance
around solder joints and within the solder resist window.
It does not appear to be flux but our customer has suggested that it could
be a fungus. The boards are shipped to China so are seeing high humidity
etc.
Has anyone ever seen anything like this and what is the solution?
We are using Multicore MF300 flux (water soluble) and are not cleaning the
boards after assembly.
Thanks,
Neil
Neil Atkinson - Quality Manager
Stadium Electronic Controls Division
Stephen House, Brenda Road, Hartlepool TS25 2BQ
#####################################################################################
Attention:
This message is for the named person's use only. It may contain confidential,
proprietary or legally privileged information. No confidentiality or privilege
is waived or lost by any mistransmission. If you receive this message in error,
please immediately delete it and all copies of it from your system, destroy any
hard copies of it securely and notify the sender. You must not, directly or
indirectly, use, disclose, distribute, print, or copy any part of this message
if you are not the intended recipient. STADIUM GROUP PLC and any of its subsidiaries
each reserve the right to monitor all e-mail communications through its networks.
Any views expressed in this message are those of the individual sender, except where
the message states otherwise and the sender is authorised to state them to be the
views of Stadium Group Plc. or one of its subsidiaries.
Although this message has been scanned by MailMarshall for known viruses and
inappropriate content, we recommend that recipients employ appropriate measures on
their systems to intercept any such material.
Thank You - Stadium Group Plc., IT Department - Tel: +44 (0)1429 266544
#####################################################################################
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|