To form a joint with a palladium finished component, the palladium has to be
dissolved into the joint. This only happens with time and temperature which
is longer and higher than those used for other metal, e.g. silver, tin,
tin/lead, finishes.
I doubt whether the flux chemistry (regardless of whether in wave or paste)
if operating with your standard process has much to do with the joint
formation with palladium unless the chemistry is sensitive to the longer
time or higher temperature. There are flux chemistries currently in use that
will 'burn out' if an incompatible profile, i.e. longer time, and/or higher
temperature is used, if that is the case then you'll need to ask your
suppliers for a material with a wider operating window. It doesn't need to
be excessively wide just less sensitive to time and temperature, some of the
chemistries developed for lead-free assembly may be useful to you.
Best regards.
Andrew Hoggan
BBA Associates Ltd
www.bba-associates.com
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|