Chris, I am confused by your question. Connector pins are either soldered or
swaged if you are talking about the wire attachment end of the pin. Swaging
then soldering on connector pins or visversa can be a disaster. Where do the
pads come into play?
Unless you can tolerate a good bit of loss at the freqs. you are talking
about, make sure that you have a solid connection. Remember that RF currents
travel on the surface of the conductors.
Ron Dieselberg
Trainer/Auditor
CMC ELECTRONICS
CINCINNATI
[log in to unmask]
-----Original Message-----
From: Chris Stack [mailto:[log in to unmask]]
Sent: Wednesday, October 03, 2001 14:36 PM
To: [log in to unmask]
Subject: [TN] pin swaging - soldering still required?
I need some advice about swaging connector pins. After they
are swaged, is
soldering still neccessary or will clamping down on the pad
make an
acceptable solder joint? The circuits they will be in are
in the 450MHz -
1GHz range.
Thanks For your help.
Chris
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using
LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with
following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following
message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources
& Databases > E-mail Archives
Please visit IPC web site
(http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|