keep in mind that dielectric strength (volts/mil) is a function of thickness. by that i mean that the dielectric strength measured on a 'thin' sample will be greater than the dielectric strength measured on a thick sample. if this is an important property, you should measure the breakdown strength on the dielectric at the thickness you intend to use.
phil
-----Original Message-----
From: Darnell, Barry (IndSys, GEFanuc, CDI)
[mailto:[log in to unmask]]
Sent: Thursday, September 27, 2001 6:56 AM
To: [log in to unmask]
Subject: [TN] Dielectric Strength
Can someone tell me the dielectric strength (how many dc volts per mil,
layer to layer) can FR-4 handle? Also, I need to create a capacitor between
two pieces of copper
on opposite sides of the board. How do I calculate the size of the copper
to achieve a given capacitance.
Thanks,
> Barry Darnell
> (864)627-8800 Ext. 217
> mailto:[log in to unmask]
> Computer Dynamics, Inc.
> Printed Circuit Board Designer
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|