Ok... Here we go again. We are experiencing solder beads found UNDER chip
components. The following questions are for all SMT assemblers (this info
would be very helpful to me):
1) Do you look for solder balls under chip devices?
2) Do you find them?
3) Do you rework this anomaly?
4) What workmanship criteria are you working to (i.e. MIL-STD-2000,
IPC-610, other)?
Thanks in advance,
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|