did your ess include vibration? i've seen fasteners fail, and the subsequent fretting in vibration caused a 'dirty' appearing surface.
phil
-----Original Message-----
From: fullname [mailto:[log in to unmask]]
Sent: Tuesday, September 25, 2001 12:34 AM
To: [log in to unmask]
Subject: [TN] Dirt on Coated Board (UC)
Some assembled boards were coated with Humiseal 1B31. After the ESS
tests at 110 degree C, dirts were found on the board and component
surfaces on both sides. I have checked the data specification on 1B31
and found that under cured enivronemnt, the coating should withstand -65
to +125 degree C.
Can someone advice me what could be the cause of this problems?
Your assistance is greatly appreciated.
Regards - Wee Mei
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|