>>> "Kathy Kuhlow" <[log in to unmask]> 09/18/01 02:32PM >>>
What type of part are you soldering? What type of flux? How old are the parts, PCB?
Please, supply more information regarding the defects being found. Include your process set-up info (speed, temp of preheats, solder dwell, angle, types of waves, nitrogen or not, etc.)