Bill,
My experience with the type ovens you describe have shown them to do an
excellent job of exhausting outgassed material and precluding redeposit on a
board or substrate surface. If it is outgassing, I would tend to believe
that you would see a difference in wire bond pull strengths as well.
Especially when comparing before/after accelerated bakes. Is this the case?
Please forgive me, but are you absolutely sure the same lot and even same
syringe/application of epoxy was used on both board types?
Bruce Misner
> ----------
> From: Bill Christoffel[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.
> Sent: Thursday, September 06, 2001 9:03 AM
> To: [log in to unmask]
> Subject: [TN] Outgassing of LPI's and Legend Inks
>
> Technetters,
>
> We are experiencing what appears to be the result of some type of
> outgassing of white legend ink.
> Details: Board design uses a white legend ink as an overcoat.
> Subsequent processing includes die attach (COB) using electrically
> conductive epoxy. Testing shows that the die attach epoxy strength (die
> shear) is greatly reduced on boards that use the white legend ink. I do
> not believe this to be a surface contaminant issue since the epoxy
> failure mode is cohesive. Epoxy cure temperature is 150C in a air
> circulating oven with a high exhaust rate. Questions - Is outgassing
> of legend inks and LPI's a probable cause? Is any information
> available regarding this ?
>
> Bill C.
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|