Peter
Ideally - do this in separate areas, although inevitibly a bottle of rework flux would mysteriously walk from one area to the other. Education will be key to success in this. Some scheme of idendifying which flux is which AND which boards are which is also essential.
There's nothing quite like a board reworked with OA flux that catches fire in a powered thermal shock oven to stink a place up.
good luck!
regards
Graham Collins
Process Engineer,
Northrop Grumman
Atlantic Facility of Litton Systems Canada
(902) 873-2000 ext 6215
>>> [log in to unmask] 09/20/01 07:51AM >>>
We use mostly OA flux for all applications, but some hardware requires RMA.
We have color-coated flux dispensers and bobbins for wire solder, and our
solder wick has no flux at all. This seems to work well.
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: PL [SMTP:[log in to unmask]]
Sent: Wednesday, September 19, 2001 3:59 PM
To: [log in to unmask]
Subject: [TN] Chemistries on production floor
Hello,
Our company will soon be introducing No-clean chemistries into our
production on certain customers. I like to know what practices are
being
applied to ensure correct handling and distinguish of OA/ No-clean
chemistries on the production floor. Any advice on process control
is
appreciated.
Does anyone have any issue with having more than one chemistries on
the
floor? E.g. identification of in-process units built with different
chemistries.
Rgds,
Peter
_________________________________________________________
Do You Yahoo!?
Get your free @yahoo.com address at http://mail.yahoo.com
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|