Barry,
This data will be in laminate manufacturers data sheets and can vary
much from one manufacturer to another. If you are wishing a precise and
constant electrical capacity, forget it. The dielectric constant can
vary much according to the manufacturer, the batch, the absorbed
humidity and the temperature. Epoxy resins do not make good capacitors
(have you heard of an epoxy capacitor as a component?) and the power
factor is very poor, to boot.
Brian
"Darnell, Barry (IndSys, GEFanuc, CDI)" wrote:
>
> Can someone tell me the dielectric strength (how many dc volts per mil,
> layer to layer) can FR-4 handle? Also, I need to create a capacitor between
> two pieces of copper
> on opposite sides of the board. How do I calculate the size of the copper
> to achieve a given capacitance.
>
> Thanks,
>
> > Barry Darnell
> > (864)627-8800 Ext. 217
> > mailto:[log in to unmask]
> > Computer Dynamics, Inc.
> > Printed Circuit Board Designer
> >
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|