TECHNET Archives

September 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Date:
Thu, 27 Sep 2001 10:45:30 +0800
Content-type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (214 lines)
Electroless Nickel / Immersion Gold - PCB plating finish.

Peter Duncan



                    "Louis, Edwin
                    @ CSE"               To:     [log in to unmask]
                    <Edwin.Louis         cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST
                    Sent by:             Aero/ST Group)
                    TechNet              Subject:     Re: [TN] White Immersion Tin
                    <[log in to unmask]
                    ORG>


                    09/26/01
                    08:34 PM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum."






What is ENIG.?

-----Original Message-----
From: Steve Kelly [mailto:[log in to unmask]]
Sent: Tuesday, September 25, 2001 3:49 PM
To: [log in to unmask]
Subject: Re: [TN] White Immersion Tin


I apologize to the Tech-net - I inadvertently sent out the wrong e-mail.

I can add some feedback on immersion tin. We have neen running for over 2
years. The process does give a very good flat solderable surface and is a
much easier process to control than ENIG. However it is very aggressive on
soldermasks and dislikes thermals. We even silkscreen before we put down
the
immersion tin so we have the freshest surface available for soldering.

Regards Steve Kelly

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Neil Atkinson
Sent: Tuesday, September 25, 2001 3:48 AM
To: [log in to unmask]
Subject: Re: [TN] White Immersion Tin


The advantages and disadvantages of immersion tin have been well covered in
the TechNet in the past so it may be worth checking the archives.

Anyway, for what it's worth here's what I have found with experience / what
I have heard.

Key advantages are it is flat, relatively cheap, easy process to install
and
control and, in my experience gives reasonable solderability even after
storage provided the boards are reasonably well packaged.

As for disadvantages, I have seen instances where the chemistry used for
the
immersion tin has attacked the solder resist and exposed copper, I'm not
sure how environmentally friendly the chemistry is (although I am sure
someone will now answer this!!).

Overall, it depends what you want, no doubt someone will say ignore it and
go for NiAu or HASL but I would say that it is a good general alternative
to
HASL and even in some cases NiAu (e.g. can carbon be used for any
contacts?).  If you haven't tried it I would say try it and use it where
the
price / performance ratio seems to be in favour of it.

It does not suffer from whisker growth because it's structure is such that
it reduces stresses in the material which cause growth (apparently!!).
However, one question which I would ask is if anyone knows whether if white
tin is put under mechanical stress e.g. by use of press fit connectors, can
it then produce tin whiskers?

One problem I have seen is with tin being slivers being produced by
press-fit connectors resulting in shorts.

Neil

Neil Atkinson - Quality Manager
Stadium Electronic Controls Division
Stephen House, Brenda Road, Hartlepool (UK) TS25 2BQ


                -----Original Message-----
                From:   Louis, Edwin @ CSE [mailto:[log in to unmask]]
                Sent:   24 September 2001 14:49
                Subject:        White Immersion Tin

                What are the advantages and disadvantages of Whit Immersion
Tin for PCBs?
                Are there dendritic growth possibilities?
                What thickness minimum should you have?

############################################################################

#########
Attention:

This message is for the named person's use only.  It may contain
confidential,
proprietary or legally privileged information.  No confidentiality or
privilege
is waived or lost by any mistransmission.  If you receive this message in
error,
please immediately delete it and all copies of it from your system, destroy
any
hard copies of it securely and notify the sender.  You must not, directly
or
indirectly, use, disclose, distribute, print, or copy any part of this
message
if you are not the intended recipient. STADIUM GROUP PLC and any of its
subsidiaries
each reserve the right to monitor all e-mail communications through its
networks.
Any views expressed in this message are those of the individual sender,
except where
the message states otherwise and the sender is authorised to state them to
be the
views of Stadium Group Plc. or one of its subsidiaries.

Although this message has been scanned by MailMarshall for known viruses
and
inappropriate content, we recommend that recipients employ appropriate
measures on
their systems to intercept any such material.

Thank You - Stadium Group Plc., IT Department - Tel: +44 (0)1429 266544
############################################################################

#########

----------------------------------------------------------------------------

-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------

-----

----------------------------------------------------------------------------

-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------

-----

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2