Peter,
Good Morning to you,
If I understand you right you want to know if you can have a depression on the secondary side of the board.
Please look at page 6-6 in your IPC 610C
Acceptable Class
* Minimum 75% fill. A total maximum of 25% depression including both secondary and primary sides is permitted
Also you will need to meet Table 6-2 on page 6-5
Basally you need a 75% fill with no more than a 25% depression on one given side.
Hope this helped
Have a good day
Nancy T.
>>> [log in to unmask] 09/24/01 05:12PM >>>
I need to nail down what an insufficient solder defect is. We are dealing
with through components.
We are seeing good solder fillets on the component side. But, there is a
concave dip 360 degrees around the lead of the secondary side of the
board. - (the solder doesn't fill completely to the top to be level with
the board.) There is a small fillet that goes around the lead 360 degrees.
This is not illistrated in IPC-A-610 wheater is it a defect. Would anyone
else consider this a defect?
Can anyone help clarify?
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|