>>> "Bogert" <[log in to unmask]> 09/18/01 04:50PM >>>
MIL-PRF-31032 is what the military currently uses in lieu of MIL-PRF-55110.
The major issue with the 31032 spec is that it has a QML whereas 55110 has a
QPL. Most of the QPL PWB manufacturers are not on the QML. This creates
problem unless your customers will authorize compliance to 31032, except for
the QML listing.
----- Original Message -----
From: "Jack Crawford" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, September 17, 2001 10:35 AM
Subject: [TN] Certfying to build military PCB's
>>> "David Klein" <[log in to unmask]> 09/17/01 09:11AM >>>
Hello All,
We are attempting to wade through all the information and determine how to
approach building for the military market. We have heard various
statements(i.e; Mil-55110 has been replaced by Mil-PERF_31032, you must
build to IPC-6012 type 3, class 3, etc). Does anyone have a definitive path
to approvals to pursue this market ?
Sincerely,
M. David Klein Sr.
National Sales and Marketing Manager
Waytec Electronics Corporation
Telephone: (434) 237-6391
Fax: (434) 237-1324
Mobile: (434) 851-6391
Website: www.waytec.com
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|