TECHNET Archives

September 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
"Estrada, Roland" <[log in to unmask]>
Date:
Tue, 18 Sep 2001 18:24:09 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Subject:
From:
Jack Crawford <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (113 lines)
>>> "Estrada, Roland" <[log in to unmask]> 09/18/01 04:42PM >>>

Good points.
A basic answer to a basic question.

Roland Estrada
Sr. Design Engineer
Electronic Packaging Group
Lockheed Martin - Missiles & Fire Control - Dallas
972-603-0416

-----Original Message-----
From: Jack Crawford [mailto:[log in to unmask]] 
Sent: Tuesday, September 18, 2001 3:38 PM
To: [log in to unmask] 
Subject: Re: [TN] Question about Coplanarity


>>> Ryan Grant <[log in to unmask]> 09/18/01 01:51PM >>>

Hi Liu, 
The definition for coplanarity comes from Geometric Dimensioning and
Tolerancing definitions and exist to prevent confusion.  You are mostly
correct in your interpretation, but be careful about re-defining coplanarity
into something more simple because that may cause confusion under different
circumstances.

For example, how do you define the lowest lead?  On a four sided QFP, each
four sides will have a single lead that is lower than all the others on that
particular row.  However, that lowest lead on one side may never touch the
"established seating plane" and therefore can not be considered the lowest
lead.

Furthermore, suppose one of the rows has all of the leads perfectly in line
with each other, but the entire row is excessively bent.  That row would be
the first to contact the "established seating plane" and become the lowest
lead, even though it would appear that row did not have the lowest lead.

From a practical standpoint. We just want to know if all the leads will sit
in solder when placed on a board.

Kind Regards

Ryan Grant
Advanced Technology Engineer
MCMS
(208) 898-1145
[log in to unmask] 


> -----Original Message-----
> From: Jack Crawford [SMTP:[log in to unmask]] 
> Sent: Tuesday, September 18, 2001 10:41 AM
> To:   [log in to unmask] 
> Subject:      Re: [TN] Question about Coplanarity
> 
> >>> lckang <[log in to unmask]> 09/17/01 08:48PM >>>
> 
> Hi Technetters!
>       According to JESD22-B108 (complanarity test for SMD), the device's
> coplanarity defined as the largest distance distance between the contact
> point of leads and the established seating plane, but when the
> estabilished seating plane is estabilished by three leads which are bend
> downwards, Is it mean that all other device leads are out of planar
> position.
>      So can I define it as vertical distance measured from the lowest
> lead?  
>      Thanks for your any input.
> 
> Best Regards,
> Liu Changkang
> 
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2