TECHNET Archives

September 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Date:
Thu, 13 Sep 2001 08:45:56 -0400
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (22 lines)
We're being asked to perform  electro migration testing on an ongoing
basis on pcbs we produce. The test required is defined as follows:
A drop of water (.5 Megohms/cm.) is dropped between 2 traces spaced .010
apart and a current of 3V DC is applied. Current leakage of no more than
30 micro amps / thou of seperation /minute must be met ???
 Is this a "standard" test and if so is a procedure defined anywhere (
IPC , MIL. etc) ?  Is it typical to perform this as a routine QC check
or is it the type of test normally performed as a qualification  test
only ?
 Any information on this would be much appreciated.
Paul Greene

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2