Hi Rick,

could be;

a) oxide on the joint

b) change in the composition of the original solder through elemental
contamination from your plating (pad/component) during reflow giving
differential freezing, resulting in a change in the surface appearance

c) the solder you've been supplied with is 'out of spec' (do you have a
spec?) and is freezing differentially

d) all of the above

e) none of the above

Best regards,

Andrew Hoggan
BBA Associates Ltd
www.bba-associates.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Rick Howieson
Sent: 09 August 2001 21:53
To: [log in to unmask]
Subject: [TN] Gold/Paste


We are seeing cloudy/grayish smt solder joints on boards with immersion gold
or soft body gold plating. Is this common???
Thanks,
Rick

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2