I've been using a Sniper system with very good results (lots of flexibility)
and following up with a Glenbrook RTX-2500 which can easily penetrate the
large heat sink BGA. I also do microscope visual inspection (approx 20-30X)
of the outer rows.
Regards,
Bruce Misner
> ----------
> From: Kathy Kuhlow[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Kathy Kuhlow
> Sent: Wednesday, August 08, 2001 2:42 PM
> To: [log in to unmask]
> Subject: [TN] BGA and X-ray
>
> <<File: TEXT.htm.txt>>
> Good Afternoon. Hope all is well with everyone. I was wondering, What
> is the preferred equipment to use for BGA rework/replacement and xray? I
> would like to know what equipment you are using and your likes/dislikes of
> the equipment.
>
> TIA for all responses.
>
> Kathy
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|