If this is for a final gold plating then we typically call out 50 to 150
micro inches for electroless nickel and then 3 to 8 micro inches of
immersion gold.
Regards,
Brent
-----Original Message-----
From: Jana L. Carraway [mailto:[log in to unmask]]
Sent: Thursday, August 16, 2001 12:20 PM
To: [log in to unmask]
Subject: [TN] Easy Thursday Question!
As we do not do manufacturing at this site, I have no technical data sheets
handy - so I need to ask a quick and easy question! (I haven't found the
answer on supplier's websites and have a couple calls into suppliers, but
you know how long that can take to get feedback - just kidding guys, I know
everyone is busy these days)
My question is: What is the typical electroless nickel deposition thickness?
I'm thinking it's around 3-5 microns. Is that correct? What range is given
on the technical literature from suppliers, if any of you guys has a tech
data sheet handy?
Thank you for your help!
Jana Carraway
Micro Systems Engineering, Inc.
Lake Oswego, Oregon
503-635-4016 ext 1180
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|