Steve mentions:
"Got pulled over by one of the inspectors this morning because we have this
little 6-pin DIP optocoupler that only goes about 65-per board..."
Hi Steve,
I'd be really careful with any sort of opto packaging issues. Optos, due to
the complex nature of their encapsulation/packaging, have more
environmetal problems than any other part type I've seen. There's
a hodgepodge of materials in there that dont "play well together"
when things go bad.
Proceed cautiously and thoroughly! Don't suppose you have any of
the reel left, you might send back for analysis? I've found QT to
be fairly responsive...
John
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|