Phosphate conversion coating! Could be brushed/sprayed on and then hosed
off when it has done its work. To hell with the pollution it will cause
to the ground underneath!
Brian
Carl VanWormer wrote:
>
> Definitely off-topic, but interesting . . .
>
> I have a friend who is making his new home out of a 727 airplane (see
> www.AirplaneHome.com <http://www.AirplaneHome.com> for details). He is
> investigating coatings he might use to "paint the house", and has rejected
> his first choice (Kapton) when he found that it deteriorates when exposed to
> UV and Oxygen (I think that was what it was). Since I've seen some amazing
> insights shared on this group, I thought I'd dangle this challenge in front
> of the group to see what happens . . . Any (and all) suggestions will be
> appreciated and investigated. Please let me know of your suggestions and
> I'll forward them to him.
>
> Thanks
>
> Carl Van Wormer
> Cipher Systems
> 1815 NW 169th Place, Suite 5010
> Beaverton, OR 97006
> Phone (503)-617-7447 Fax (503)-617-6550
>
> p.s. here's a snippet from my last contact with the airplane/home owner:
> Hot dog, thanks very much. I've always been very fond of RTVs - they seem
> more stable than any conventional paint, or any other coating short of
> Teflon. I've never in my life seen any evidence of any form of
> deterioration
> of RTVs, and they've been around since I was a kid. I've always thought
> they'd make a great roof coating for my mobile home (back when maintenance
> of
> the structure would've been justified) or the freight vans.
>
> The timing is quite good too in that I've been thinking about coatings
> again.
> I've been pressure washing again in the last few days, and I've noted that,
>
> while the color coats often flake off, the chromates don't, although they
> can
> bleed off. That is, the chromates seem to form a chemical bond with the
> aluminum, whereas the paint just forms an adhesive bond, which, like all
> adhesive bonds, is unreliable. When the pressurized water is forced onto
> the
> chromate at its most aggressive (with the wand within a cm or two of the
> surface), the chromate sometimes get fainter and fainter as if they're being
>
> abraded off. But they never peel. That's impressive.
>
> And that's what I'd like in a coating - a true chemical bond, so that it's
> literally part of the metal, not just a layer over the metal. Well, that,
> plus absolute immunity to UV, chemical weathering, and every other factor
> that makes a coating just plain perfect.
>
> Teflon's been on my mind too. It's extremely stable of course. But I'm not
>
> sure what the nature of it's bond is, or what the economics are - I need to
> look into it.
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|