James,
We use a "b" staged adhesive every day to repair lifted pads and conductors
in our shop. The particular material we use is a Phenolic Butral film
adhesive .0018" (.046 mm) thick. It's cured at 475°F (246°C) for 30 seconds.
You can get a little more info off our web site at
www.circuittechctr.com/products/115-2600.htm.
Contact me off line an I'll send you a sample.
Jeff Ferry
CEO
Circuit Technology Center, Inc.
www.circuittechctr.com
[log in to unmask]
978-374-5000
Sign up for our Free E-mail Newsletter at:
www.circuittechctr.com/general/free_email.htm
On Fri, 3 Aug 2001 14:52:41 -0400, James W. High <[log in to unmask]>
wrote:
>Is it possible to purchase "b" stageable epoxy for general use? I've only
>seen this term used when refering to prepregs. If there are any specially
>formulated epoxies available, please mention manufacturers and part
numbers.
>
>
>James W. High
>NASA Langley Research Center
>Mail Stop 390
>Hampton, VA 23681-2199
>
>757-864-5416 (Phone)
>757-864-8092 (Fax)
>Email: [log in to unmask]
>
>---------------------------------------------------------------------------
------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
>Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>---------------------------------------------------------------------------
------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|