Conversely Delco has been making flipchips for ever....
Mike
----- Original Message -----
From: "Werner Engelmaier" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, August 01, 2001 9:17 PM
Subject: Re: [LF] Eutectic alloys?????
> Hi,
> I am not so sure that the automotive industry is at the forefront of
> soldering technology--only 2 years ago one of the Detroit Big 3 had
to recall
> 2 years worth of SUVs because 60/40 SJs on CEM-1 [!?] PCBs for the
windshield
> wiper controls under-the-hood failed well within the warranty
period. CEM-1
> not only grossly thermally expands, but swells on H2O-absorption,
and the bad
> housing design caused the PCBs to warp.
>
> Werner Engelmaier
>
> --------------------------------------------------------------------
-------------
> Leadfee Mail List provided as a free service by IPC using LISTSERV
1.8d
> To unsubscribe, send a message to [log in to unmask] with following
text in
> the BODY (NOT the subject field): SIGNOFF Leadfree
> To temporarily stop delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> --------------------------------------------------------------------
-------------
>
---------------------------------------------------------------------------------
Leadfee Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|