We had this design and did not like it despite of fact it saved a lot of PBB
space. Problem was , especially for small chip packages ( 0603) that volume
of vias barrel is comparable to volume of solder joint and this vias was
"steeling" solder from solder joint accidentally ( during wave soldering).
Result - insufficient or even missing solder joint.
We do not have this layout design anymore ..
Regards
Vit Sklenar MGE4VS
T: (61 3)9541 7734 F: (61 3) 9541 3909
e-mail work: [log in to unmask]
e-mail home: [log in to unmask]
> Robert Bosch (Aust) ,
1555 cnr.Centre and McNaugton Road,
> Clayton , VIC 3169, Australia
>
>
> -----Original Message-----
> From: Ken Patel [SMTP:[log in to unmask]]
> Sent: Thursday, August 09, 2001 4:53 AM
> To: [log in to unmask]
> Subject: [TN] VIAS in pads...
>
> Assemblers,
> How robust is the VIA in the pad technology now? Can someone share the
> process of handling board that has vias in pads?
>
> Most of our boards have VIAS in the pads and there is no way out.
>
> re,
> Ken Patel
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|