Cathy
Ionic contamination as an absolute value is totally meaningless with
"no-clean" chemistry. The first half of your question is therefore
irrelevent. The second half can be achieved, depending on conditions,
but I question its relevence, also.
Brian
Cathy Killen wrote:
>
> Hi everyone,
> Can a no-clean process achieve ionic contamination <1.5ug cmsq according to
> IPC TM-650 2.3.25 and a surface resistance > 5 X 10 (power of 8) according
> to IPC TM-650.2.6.3.3?
> If you believe it can be achieved, how?
> How could you confirm it as an ongoing process control?
> Cathy Killen
> Training Instructor
> [log in to unmask] <mailto:[log in to unmask]>
> An Oasis of Training Excellence
> * 028 38314305
>
> DISCLAIMER
> 1. The information contained in this E-mail is confidential.
> It is intended only for the stated addressee(s) and access to it by any
> other person is unauthorised.
> If you are not the addressee, you must not disclose, copy, circulate or in
> any other way use or rely on the information contained in this E-mail. Such
> unauthorised use may be unlawful. If you believe that you have received
> this E-mail in error, please inform us immediately and delete it and all
> copies from your system.
> 2. The views expressed in this E-mail are those of the author, and do
> not represent the views of Smtek Europe., its associates or subsidiaries,
> unless otherwise expressly indicated. In the avoidance of doubt, the
> insertion of the name Smtek Europe., its associate or subsidiary under the
> name of the sender may constitute an express indication that the views
> stated in the Mail are those of the named company.
> 3. Please note it is your responsibility to scan this E-mail for
> viruses.
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|