3M Adhesives do these in the UK, they use a sub-contractor who does all the
cutting who they have very close links with.
For a more radical approach, does anyone out there have experience of using
aluminium backed laminate as a replacement for this?????
Neil Atkinson
-----Original Message-----
From: Kane, Joseph [mailto:[log in to unmask]]
Sent: 28 August 2001 16:53
Subject: Sheet Adhesive Suppliers
Our supplier for epoxy sheet adhesives has significantly increased
prices, and I'd like to look at alternative sources.
We use this stuff for bonding ladder-style aluminum heatsinks to
PWB's. The types that we use are either glass cloth or Kapton
film covered with epoxy, total thickness from .004" to .009". We
cut material on a programmable x-y machine that looks a lot like
a plotter, but with a blade instead of a pen. Cure is with heat and
pressure, either in a fixture and oven, or with a vacuum bag and
platen press.
We like dry film better than screen printing or dispensing liquid
adhesive because it's a lot less messy, bondline thickness is very
repeatable, material doesn't squeeze out when fixtured, and there
is no smear when aligning the heatsink with the board.
Anyone use Arlon materials for something like this? Other sources?
#####################################################################################
Attention:
This message is for the named person's use only. It may contain confidential,
proprietary or legally privileged information. No confidentiality or privilege
is waived or lost by any mistransmission. If you receive this message in error,
please immediately delete it and all copies of it from your system, destroy any
hard copies of it securely and notify the sender. You must not, directly or
indirectly, use, disclose, distribute, print, or copy any part of this message
if you are not the intended recipient. STADIUM GROUP PLC and any of its subsidiaries
each reserve the right to monitor all e-mail communications through its networks.
Any views expressed in this message are those of the individual sender, except where
the message states otherwise and the sender is authorised to state them to be the
views of Stadium Group Plc. or one of its subsidiaries.
Although this message has been scanned by MailMarshall for known viruses and
inappropriate content, we recommend that recipients employ appropriate measures on
their systems to intercept any such material.
Thank You - Stadium Group Plc., IT Department - Tel: +44 (0)1429 266544
#####################################################################################
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|