James,
Only from what I've read (no practical experience of this problem), it can
be caused by an inappropriate solder mask, especially if you're wave
soldering after CR. Which solder mask are you using? Is your problem a
regular feature, and does it occur on all chip components or just some (is
there a pattern)? What processes are you using? Is the board double sided?
Regards
Pete Duncan
"Marsico, James"
<James.Marsico@D To: [log in to unmask]
P.AIL.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Sent by: TechNet Subject: [TN] soldr balls
<[log in to unmask]
>
08/15/01 03:34
AM
Please respond
to "TechNet
E-Mail Forum.";
Please respond
to "Marsico,
James"
Here's a relatively basic SMT question, but we've haven't experienced this
before. We're seeing solder balls under (way under, in the center) chip
components. Any recommendations?
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|