True: I have a copy of an MSDS for water issued a few years ago by a well
known chemical house, it follows the usual format including what to do
following skin and eye contact (flush with water.....).
Mike Fenner
Indium Corporation of Europe
T: + 44 1908 580 400
F: + 44 1908 580 411
M: + 44 7810 526 317
W: www.indium.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Graham Naisbitt
Sent: Friday, July 20, 2001 11:00 AM
To: [log in to unmask]
Subject: Re: [TN] White residue from conformal coating
Hans
Hope you will excuse me for butting in but - health concerns?
Water will kill you if you drink too much of it! Guess it should be banned
in Europe and California?
Regards, Graham Naisbitt
[log in to unmask]
http:// www.concoat.co.uk <http://www.concoat.co.uk>
For instant access to Product Data Sheets register on the Tech-Shot area of
http:// www.concoat.co.uk <http://www.concoat.co.uk>
Concoat Limited
Alasan House, Albany Park
CAMBERLEY GU16 7PH UK
Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227
Mobile: +44 (0)79 6858 2121
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Hans Hinners
Sent: Thursday, July 19, 2001 09:19
To: [log in to unmask]
Subject: Re: [TN] White residue from conformal coating
Hey Doug,
Does MPK have the same health concerns as MEK?
Hans
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Process Engineer
Toppan Electronics, Inc.
770 Miramar Road
San Diego, CA 92126
(858) 695 - 2222 ext. 241
(858) 695 - 6823 fax
[log in to unmask]
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, July 19, 2001 5:38 AM
To: [log in to unmask]
Subject: Re: [TN] White residue from conformal coating
Graham,
Thanks for the insights on the "blush" phenomena. How interesting that it
comes up in the same discussion as your "work naked bonus".
Is there any link between the type of solvent in the coating and blush, or
is it exclusively humidity related? One project that has been suggested
for me is to replace the toluene and xylene we use as acrylic thinners with
methyl propyl ketone. If such a switch were made, would you expect a
greater or lesser susceptibility to blush, or is it immaterial (no pun
intended).
Doug Pauls
Rockwell Collins
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|