Kathy,

is the white residue on, in, or under the conformal coating?

could be moisture-related.

Hans Shin
Pacific Testing Laboratories, Inc.
www.pacifictesting.com

-----Original Message-----
From:   Kathy Kuhlow [SMTP:[log in to unmask]]
Sent:   Wednesday, July 18, 2001 10:24 AM
To:     [log in to unmask]
Subject:        [TN] White residue from conformal coating

What causes white residues after conformal coating?  The coating is an acrylic and after the first coat there appears to be a white residue and after the 24 hour cure the coating appears very dull and still has some of the white residues.  The residues almost look like water flux residue but it isn't.  The supplier that the coating was purchased from says it is strictly humidity related and only a cosmetic issue.  There is no visible loss of adhesion.  The solder mask is a LPI matte finish.  Can this be part of the problem?  
 << File: TEXT.txt >>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives