Hi, Shou Kai,
We had a CPU card designed and made for us in the States, and it carries
BGA's - 256 and 388 pin devices. This board has an ENIG finish to provide
adequate flatness for the BGA's - the finish is 4.5 microinches hard gold
over 150 microinches Nickel on a 12 layer FR4 board - quite a thick Nickel
layer, I think, but that's what the designers specified.
Soldering was a concern to me too, with visions of high melting point
solder with silver content and risks of frying dies trying to achieve a
good soldering temperature. But we tried a eutectic solder paste (63/37)
specially formulated for fibre optics work and it worked very well. Wetting
was good, solder joints were properly formed. Peak soldering temperature
was 218 deg C for about 16 seconds, bringing the centre pins of the BGA's
up to 205 deg C.
If your board is in good condition, you should have no problems.
Pete Duncan
Shoukai Zhang
<skzhang@HUAW To: [log in to unmask]
EI.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Sent by: Subject: [TN] PCB surface finishes
TechNet
<[log in to unmask]
ORG>
07/11/01
05:27 PM
Please
respond to
"TechNet
E-Mail
Forum.";
Please
respond to
Shoukai Zhang
Dear TechNetters:
As we know that the preferred metal surface finishes are HASL, EN/IG
(Electroless Nickel and Immersion Gold, and OSP etc.
It's reported that EN/IG(also called immersion gold) suface may lead
unreliable solder joint for BGA component, and suggest do not use
immersion gold for designs that have BGAs.
Please give your advices.
Thanks with best regards,
Zhangshoukai, PE, Huawei Technologies.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|