I highly recommend a book by George Harman "Wire Bonding in
Microelectronics" Materials. Processes, Reliability and Yield.
IMHO, For Thermosonic Gold Ball Bonding : 45 microinches of
Electrolytic Soft Au. over 155 microinches of Ni.
If you are doing Al. Ultrasonic Wedge Bonding, your material
possibilities are increased, (immersion Au. etc.)
Bill C.
NorLux Corp.
-----Original Message-----
From: Buscomb, Scott [mailto:[log in to unmask]]
Sent: Monday, July 02, 2001 9:36 AM
To: [log in to unmask]
Subject: [TN] Specs for Wire Bond Pads
I am looking for information on specifying a gold plated surface for
wire
bond pads, specifically plating, surface roughness and contamination.
Does a
standard industry spec exist? Is there an authoritative text on the
subject?
Thanks in advance.
Scott Buscomb
------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|