IPC-A-610 states lead lengths and trimming required for Classes 1, 2 & 3 of
board. Normally, lead protrusions are cropped to 1mm to 1.5mm max. There
are other associated factors like clinching or non-clinched connections adn
lead lengths required for those, board thickness considerations, etc.
Rgds
Another Peter (Duncan)
PL
<ppwlee@YAHOO To: [log in to unmask]
.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Sent by: Subject: [TN] Lead protrusion
TechNet
<[log in to unmask]
ORG>
07/12/01
02:26 PM
Please
respond to
"TechNet
E-Mail
Forum.";
Please
respond to PL
Hello,
Does anyone know what is the standard used for prepping
the leads for through-hole boards?
What are the critical parameters one should consider
when determining the amount of trimming on the leads?
Rgds,
Peter
_________________________________________________________
Do You Yahoo!?
Get your free @yahoo.com address at http://mail.yahoo.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|