Hi,
We use Hot-melt product or adhesive foam tapes for gluing the components
on the surface.
Best regards,
Ketan Bhatt.
----- Original Message -----
From: "COWEN,MARC (A-Scotland,ex1)" <[log in to unmask]>
Sent: Wednesday, July 11, 2001 3:43 PM
Subject: PTH soldered onto smt pad
> Hi All,
>
> We currently have a modification to a PCA where we have added a capacitor.
> Unfortunately the only capacitor suitable for this is a through hole
device.
> We have therefore asked our supplier to form the legs as follows:
>
>
>
>
>
>
>
>
>
>
>
> We have had instances where the solder on the left hand leg has not been
> sufficient, the leg has come loose and this has worked like a spring. Also
> the RTV compound we have also found to be unreliable.
>
> Could some-one please advise of the following:
>
> 1. Is there a better adhesive to use instead of RTV compound?
> 2. Is there a quick and easy way for an inspector to check the solder
> joint without placing undue stress on the capacitor legs or the solder
> joint? We currently asking inspectors to "gently" try to move the leg
while
> looking at the solder fillet through a microscope to see if there is a
> fracture.
>
> Thanks for your help.
>
> Marc.
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|