TechNetters, I'd appreciate comments on contaminant analysis of a wave
solder pot. We had been sending a sample out for analysis (type "C" I
think it is, by the mil spec) once per month. Now the solder supplier is
telling me that once every six months is more than enough. I've been
taking the contaminant data and plotting Q charts (for short-run SPC the
modern way, as I've been mentioning in this forum) with the monthly data.
What has been your practice and recommendation?
At the moment, it is hard for me to feel comfortable with a twice-yearly
analysis of what seems to me to be an important material in our
manufacturing process. Lou Hart
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|