Hello Paul,
Have you tried to download "Fred's Tip Cartridge Picker" from
http://www.metcal.com/tips/1.3.4.htm ?
It's a little Excel document (40kb compressed) and after you have choosed
the geometry of the components, you get the suggestion of the metcal tip
that should be used.
Approx. temperature range of the metcal tips should be:
500 series around 285 degrees celsius
600 series around 315 degrees celsius
700 and 1100 around 370 degrees celsius.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2