Rudy
The non-electroless copper processes eliminate the chemical attack on the
aluminum during electroless copper process, but:
The Shadow or Black Hole processes work by coating all surfaces with a
conductive coating and then removing the conductive coating from all of the
metallic surfaces.
You are then back to trying to plate the aluminum with the acid copper
plating process.
Phil
---------------------------------------------------------------------------------