Douglas,
The solder paste that refer from Multicore is SN63CR32 and qualified for
SDT-J-004 with an ROL0 designation.
Regards,
Douglas Pauls
<[log in to unmask] Para: [log in to unmask]
KWELL.COM> cc:
Enviado por: TechNet Asunto: Re: [TN] ATTN: No
<[log in to unmask]> Clean Solder Users
14/06/01 12:13 p.m.
Por favor, responda
a "TechNet E-Mail
Forum."; Por favor,
responda a dopauls
>> I'm beginning an evaluation of no clean solder pastes.
I was wondering what pastes fellow technetters are using, and
their production environment.>>
James,
A few months ago, we finished a big evaluation of low solids solder pastes.
We settled on Indium SMQ92J and Alpha Metals UP-78M as our two preferred
pastes. When I was at CSL, I evaluated both materials for several clients
and it always had excellent residue characteristic by ion chromatography,
as well as excellent SIR performance. If you are looking at materials to
consider, I would also add Kester 256GS to your list. It has also done
very well in my evaluations. Multicore also makes a good low solids paste,
but the exact designation escapes me for now (something in their X-32 or
X-33i series, if I recall). I am sure many of the other paste
manufacturers have decent low solids pastes, but my experience with those
is limited.
Look for a J-STD-004 qualified paste, with an ROL0 designation. If you are
going to no-clean assembly, avoid halides like the plague. A plus would be
if the paste is also Bellcore compliant. I can talk more off-line, if'n ya
want.
Doug Pauls
Rockwell Collins
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|