Hi All,
As I told Jim offline, this is quite possible (many are conformal coating
without cleaning now), but is dependent upon the flux, coating, and coating
application. If anyone would like I can send to them a paper on testing
various (AIM) paste and liquid fluxes with various coatings.
Best regards,
David Suraski
AIM
T: 800-CALL-AIM / 401-463-5605, F: 401-463-0203
www.aimsolder.com
> -----Original Message-----
> From: West, Jim [mailto:[log in to unmask]]
> Sent: Wednesday, June 27, 2001 9:01 AM
> To: [log in to unmask]
> Subject: [TN] Conformal coating
>
>
> Hi,
>
> Do boards have to be cleaned before you apply conformal coating? Does it
> depend on what type of flux is used? Example would be no-clean flux, you
> can apply conformal coating over it right?
>
> Thanks,
> Jim
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|