A dynamic solder pot is generally used for pre-tinning gold plated parts.
The solder movement actually "washes" away the gold.
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: Anderson, Greg (IndSys, GEFanuc, NA)
[SMTP:[log in to unmask]]
Sent: Wednesday, June 20, 2001 9:15 AM
To: [log in to unmask]
Subject: Re: [TN] flowing solder pot
Jim,
Why do you want this to be "flowing"? If you really want it
on the
cheap, couldn't you use a small static pot and skim the dross out of
the way
when you tin? There are many available at very low cost (and low
energy to
run, low dross production).
Greg Anderson
Senior Advanced Manufacturing Engineer
GE Fanuc Automation
Charlottesville, VA 22911
Phone: 804-978-5181
FAX: 804-978-5898
e-mail: [log in to unmask]
-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]]
Sent: Wednesday, June 20, 2001 8:48 AM
To: [log in to unmask]
Subject: [TN] flowing solder pot
Hello Technet...
I'm looking for a small (cheap) flowing solder pot to do occasional
hand
pre-tinning. Any suggestions?
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|