Hello,
We have CM's that use no-clean solder paste on our PCB's. We have not given
the CM any spec other than that it be approx. 60/40 tin-lead. In house,
however, for hand assembly we have always used solder such as Kester "44" RA
core solder. We're working on a new OEM product and the customer has
expressed concerns about mixing the two on the same PCB. We also use a
safety wash board cleaner.
Any thoughts or concerns that we should address?
Genny Gibbard (mailto:[log in to unmask])
Product Transition and Support
Wavecom Electronics Inc.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|