Is it common to see values of capacitors drift after temperature cycling? I
had a 15% ICT fallout on some caps after 48 hrs temperature (85deg)
cycling.
The values drifted @+/- 11% from their nominal. The component specs allow a
+/- 10%, but I am curious why the moderate temperature cycling would cause
a 15% failure rate for capacitor value drifting when they were tested on
the ICT second time around.

The ICT parameters/set up did not change and I had 100% ICT pass rate first
time around.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2