TECHNET Archives

June 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
Date:
Fri, 1 Jun 2001 14:02:33 -0500
Content-Type:
multipart/mixed; boundary="=_673D46C5.A5C4A804"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Kathy Kuhlow <[log in to unmask]>
Parts/Attachments:
text/plain (291 bytes) , TEXT.htm (640 bytes)
IMHO exposed copper needs to be repaired.  I have seen instances where the solder mask continues to flake off after wave soldering and starts to affect reliability.  Not to mention the risks of  fluxes entrapment or the oxidation when the copper is left exposed to the elements.  

Kathy 



<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN"> <HTML><HEAD> <META content="text/html; charset=iso-8859-1" http-equiv=Content-Type> <META content="MSHTML 5.00.2614.3500" name=GENERATOR></HEAD> <BODY style="FONT: 10pt Haettenschweiler; MARGIN-LEFT: 2px; MARGIN-TOP: 2px"> <DIV>IMHO exposed copper needs to be repaired.&nbsp; I have seen instances where the solder mask continues to flake off after wave soldering and starts to affect reliability.&nbsp; Not to mention the risks of&nbsp; fluxes&nbsp;entrapment or the oxidation when the copper is left exposed to the elements.&nbsp; </DIV> <DIV>&nbsp;</DIV> <DIV>Kathy </DIV></BODY></HTML>