TECHNET Archives

June 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Hann Pang <[log in to unmask]>
Date:
Fri, 8 Jun 2001 08:11:48 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (114 lines)
Pete,

3M has a range of thermally conductive tapes and pads for such purposes,
the latest product is a double sided tape, 5, 10 or 15 mils thick with
excellent wet out and adhesion. thermal conductivity is about 0.6 W/mK.

If higher thermal condutivity around (2.5-3W/mK) is needed, there are
conductive pads but these has pretty low adhesion values and are thicker.
Let me know if you need more info.

Best regards,
Hann




Joyce Koo <[log in to unmask]> on 06/08/2001 07:24:07 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to Joyce Koo <[log in to unmask]>


To:   [log in to unmask]
cc:    (bcc: Hann Pang/US-Corporate/3M/US)
Subject:  Re: [TN] Thin Thermal Pad Materials



try AI Technology, use paste with filler (thermal set)...
www/aotechnology.com
good luck.
                     jk

-----Original Message-----
From: <Peter George Duncan> [mailto:[log in to unmask]]
Sent: June 7, 2001 10:33 PM
To: [log in to unmask]
Subject: [TN] Thin Thermal Pad Materials


Hi, Everyone,

We are working on a conduction-cooled VME SMT board design for an
avionics
application. It requires a 7 degree C thermal gradient from Chip die at
the
board centre to card the edge, which may be impossible, but we're trying
so
I need your advice.

I'm looking for a highly efficient thermal material 0.30mm thick +/-
0.03mm
and a material 0.15mm thick +/- 0.03mm to fill component air gaps and
other
material interfaces. It should have double-sided adhesive, and require
an
absolute minimum attachment pressure.

I cannot find any materials anywhere, myself, that aren't 0.25mm or
0.5mm
or thicker. And there's nothing as thin as 0.15 finished thickness even
in
thermal tapes. We don't want to use greases or anything silicone either.

Any ideas, anyone, as to where I might find a material souce to meet
such
requirements?

TIA for your ever-wonderful ideas.

Pete Duncan

------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2