Is this talc used as a lubricant between insulated conductors in
multi-cored cable? Quite often this is French Chalk and not talc, which is
a different mineral.
Pete Duncan
Douglas Pauls
<[log in to unmask] To: [log in to unmask]
KWELL.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Sent by: TechNet Subject: Re: [TN] Talcum powder on wires
<[log in to unmask]>
06/07/01 08:25 PM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to dopauls
Good day, does anyone know of complications or issues that would come about
from talcum powder being present on a wire harness that is hand soldered to
an electronics board?
For instance would the talcum powder affect the solderability of the wires?
Could the talcum powder react with rosin flux?
*Jason, I don't know that you would have a big problem with solderability,
but talcum powder is usually loaded with ionic residue, such as chloride
and sulfate. I would be concerned that the powder would get on the board
and cause corrosion. Since talcum powder is largely mineral, it could
react with rosin flux, but I have no idea what the resultant combination
would look like. Will you be cleaning the board/harness combination?
Doug Pauls
Rockwell Collins
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|