TechNetters,
Is it possible to clean assemblies containing socketed components in an
aqueous cleaner? We have an in-line cleaner with 2% saponifier for
cleaning after surface mount reflow (water-soluble paste) and after wave
solder (water-soluble flux).
My concern is with assemblies that have had components reworked with
water-soluble flux after socketed parts have been installed. The cleaning
procedure in IPC-7721, 2.2, recommends use of an automated cleaner, and
provides instructions on hand-cleaning.
Many thanks for any comments.
Lou Hart
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|