TECHNET Archives

June 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Douglas Pauls <[log in to unmask]>
Date:
Fri, 1 Jun 2001 07:58:43 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (23 lines)
Jim,
There is more at stake than just solderability.  Finger salts and oils can
create corrosion and metal migration problems when mixed with the humidity
in the air.  In addition, you can have problems with conformal coat
adhesion because of hand oils, especially if you use those anti-static hand
lotions.  We don't worry about it too much at Rockwell because all of our
boards go through a cleaning prior to conformal coating.  But, as we
transition to no-clean assembly, we know that handling will be a issue an
we will have to train our operators to work on an "edges only" basis.

Doug Pauls
Rockwell Collins

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2