TECHNET Archives

June 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
Joyce Koo <[log in to unmask]>
Date:
Tue, 5 Jun 2001 10:12:58 -0400
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Parts/Attachments:
text/plain (175 lines)
Kevin,
the problem is: when you complete your test (i can think about many
other tests, such as humidity/bias...because it is polyimide, not FR4),
are you sure the board still can be used for the field?...  He is only
having on the rework board, hopefully, he only need to deal with one or
two (not many, otherwise, we are dealling with QA problem)....How much
effort you should put in for unique one or two, possibly due to
non-compliance of procedures....(too many "ifs")...Resistivity test at
current stage will be a "pass"...the trick is, who knows what is the
impact at end of life of the product...(don't like to deal with
polyimide...if steve know about his vendor product, such as weight loss
value, he may have some guesstimate of the quality v.s. the measling
impact)...
 
jk

-----Original Message-----
From: PERALTA, Kevin (BREA) [mailto:[log in to unmask]]
Sent: June 5, 2001 9:41 AM
To: [log in to unmask]
Subject: Re: [TN] Measling...



Hey Joyce! Don't go to far out there. Remember "Inspect to Accept"!
Since there is only "Acceptable" criteria mentioned in the 610 document,
I would suggest to Steve to perform a dielectric resistance test to ease
his mind. Unless heat is going to be applied to the board again, the
condition probably won't progress.

Kevin L. Peralta 
Senior Quality Systems Analyst 
TRW Aeronautical / Lucas Aerospace 


-----Original Message----- 
From: Joyce Koo [ mailto:[log in to unmask]
<mailto:[log in to unmask]> ] 
Sent: Tuesday, June 05, 2001 5:35 AM 
To: [log in to unmask] 
Subject: Re: [TN] Measling... 


I am no so sure...Steve is using polyimide board, which most likely is 
for high reliability usage (not off the shelf items for commercial 
usage)...I would not use it if it is for avionics (measling cross the 
sky is scary...it may infect the stars...)..jk 

-----Original Message----- 
From: <Peter George Duncan> [ mailto:[log in to unmask]
<mailto:[log in to unmask]> ] 
Sent: June 4, 2001 10:23 PM 
To: [log in to unmask] 
Subject: Re: [TN] Measling... 


No. The measling looks quite minor and doesn't come close to other 
traces 
or pads. Unless I'm mis-judging the scale of the picture, the affected 
area 
isn't carrying high power either, so I don't see that there's a problem.


Pete Duncan 




                    "Stephen R. 
                    Gregory"             To:     [log in to unmask] 
                    <SteveZeva@AO        cc:     (bcc: DUNCAN Peter/Asst

Prin Engr/ST Aero/ST Group) 
                    L.COM>               Subject:     [TN] Measling... 
                    Sent by: 
                    TechNet 
                    <[log in to unmask] 
                    ORG> 


                    06/05/01 
                    02:58 AM 
                    Please 
                    respond to 
                    "TechNet 
                    E-Mail 
                    Forum."; 
                    Please 
                    respond to 
                    SteveZeva 






Hi ya'll! 

I took a few days off last week, and came back to be confronted with 
some 
boards that have been measled from rework... 

Go to: http://stevezeva.homestead.com/index.html
<http://stevezeva.homestead.com/index.html>  to take a peek. 

The boards are polyimide, and it obviously appears that there was too 
much 
heat used when they were reworked...also they may have not been baked 
prior 

to the rework...I was told that they were, but you know how that goes. 

I know what the -610 says about it, it says it's acceptable as long as 
the 
assembly performs as specified. There isn't any burns or anything around

any 
of the barrels, just the measles...and it's only on one 14-pin DIP 
location. 
Would any of you have any REAL hesitation about accepting this assembly?


Thanks! 

-Steve Gregory- 

------------------------------------------------------------------------

--------- 
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d 
To unsubscribe, send a message to [log in to unmask] with following text 
in 
the BODY (NOT the subject field): SIGNOFF Technet 
To temporarily halt delivery of Technet send the following message: SET 
Technet NOMAIL 
Search previous postings at: www.ipc.org > On-Line Resources & Databases

> E-mail Archives 
Please visit IPC web site ( http://www.ipc.org/html/forum.htm
<http://www.ipc.org/html/forum.htm> ) for 
additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700

ext.5315 
------------------------------------------------------------------------

--------- 

------------------------------------------------------------------------
--------- 
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d 
To unsubscribe, send a message to [log in to unmask] with following text
in 
the BODY (NOT the subject field): SIGNOFF Technet 
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL 
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives 
Please visit IPC web site ( http://www.ipc.org/html/forum.htm
<http://www.ipc.org/html/forum.htm> ) for additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315 
------------------------------------------------------------------------
--------- 

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2