Bruce,
We've been using immersion silver since 1997. Most of our fabricators have
implemented the immersion silver plating process because it is our surface
finish of choice.
The best source of information is probably the 1998-1999 papers presented at
the IPC National Conferences on Solderability and Surface Finishes. There
are papers from Lucent, Intel, and MacDermid. We also presented a paper at
SurFin 2000 in Chicago.
Why do you want to switch from immersion tin to immersion silver? Did you
have problems with immersion tin?
Regards,
George
George M. Wenger, DMTS Bell Laboratories Princeton
Supply Network Solutions
PO Box 900, Princeton NJ 08542-0900
Route 569 Carter Rd., Hopewell, NJ 08525
(609)-639-2769 (Office), 3210 (Lab), 2346 (Fax)
[log in to unmask]
-----Original Message-----
From: Bruce Bryla [mailto:[log in to unmask]]
Sent: Friday, June 29, 2001 6:41 AM
To: [log in to unmask]
Subject: [TN] Immersion Silver
I am looking to transition from immersion tin to immersion silver for PWB's.
I would be interested in receiving comments/information from users and their
experiences, both positive and negative.
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|