Hello Jim,
In my own experince, in not necesary to wash the PCB before apply a
conformal coating (otherwise you're using a washable flux), only be careful
if you are using a flux with visible flux residues or if you don't
activated enough your flux.
If you are applying a conformal coating UV curable, heat produced by UV
oven could actived your flux residues and have delaminations of your
conformal.
I hope this advice could be useful for you,
Regards,
Mario.
"West, Jim"
<jwest@NEXERG Para: [log in to unmask]
Y.COM> cc:
Enviado por: Asunto: [TN] Conformal
TechNet coating
<[log in to unmask]
ORG>
27/06/01
11:00 a.m.
Por favor,
responda a
"TechNet
E-Mail
Forum."; Por
favor,
responda a
"West, Jim"
Hi,
Do boards have to be cleaned before you apply conformal coating? Does it
depend on what type of flux is used? Example would be no-clean flux, you
can apply conformal coating over it right?
Thanks,
Jim
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|