I wouldn't, provided increased magnification was used, as a referee, to
visually ensure no damage has occurred to any pads of the IC (lifted edges,
delamination, etc.)
Ed
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Monday, June 04, 2001 2:58 PM
To: [log in to unmask]
Subject: [TN] Measling...
Hi ya'll!
I took a few days off last week, and came back to be confronted with some
boards that have been measled from rework...
Go to: http://stevezeva.homestead.com/index.html to take a peek.
The boards are polyimide, and it obviously appears that there was too much
heat used when they were reworked...also they may have not been baked prior
to the rework...I was told that they were, but you know how that goes.
I know what the -610 says about it, it says it's acceptable as long as the
assembly performs as specified. There isn't any burns or anything around any
of the barrels, just the measles...and it's only on one 14-pin DIP location.
Would any of you have any REAL hesitation about accepting this assembly?
Thanks!
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|