TECHNET Archives

June 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Bissonnette, Jean-Francois" <[log in to unmask]>
Date:
Tue, 19 Jun 2001 09:28:27 +0100
Reply-To:
Alan Brewin <[log in to unmask]>
Subject:
From:
Alan Brewin <[log in to unmask]>
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; charset="iso-8859-1"
Organization:
Concoat Ltd
MIME-Version:
1.0
Parts/Attachments:
text/plain (76 lines)
Jean Francois,

Blushing is generally caused by high humidity.  It is usually worst in spray
applications, but can become an issue in dipping/brushing applications as
well.

Essentially, as the solvent starts to flash-off, the evaporation causes
cooling (cf. acetone on your hand!), which then causes some of the saturated
moisture vapour to be condensed onto and into the coating.  Atomisation
causes more cooling and hence greater problems with blushing.

You could try adding a retarder solvent, but a much better solution would be
to try and reduce your humidity.  You could try using a portable
de-humidifier and held-held probe to try and maintain a max RH of about 60%,
but aim for 40%.

Hope this helps,

Best Regards,

Phil Kinner
(Masquerading as Alan Brewin!)

----- Original Message -----
From: Bissonnette, Jean-Francois
To: [log in to unmask]
Sent: 18 June 2001 16:35
Subject: [TN] Conformal coating: white haze


This is a question for all the conformal coating specialists of this
world.

We're experiencing some problems with the application of conformal coating
in high humidity
conditions.  Just after the application is finished, some kind of white haze
appears in the coating.
It disappears a little be during curing but some of it stays.  The finish of
the coating is then a little
less smooth and shinny than normal.

In order to avoid excess of humidity, the boards are pre-heated for 24h.
The coating used is
acrylic.

Anyone knows what causes this?


Jean-François Bissonnette
Contrôle de la Qualité, Électronique
Quality Control, Electronics
Vapor Canada Inc.
10655 Henri-Bourassa O.
St-Laurent, Qc
H4S 1A1
(514) 335-4200 Ext: 2021



WABTEC CORPORATION CONFIDENTIALITY NOTE
The content contained in this e-mail transmission is legally privileged and
confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly prohibited.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2